SPECIFICATIONS
MODEL |
Graphene Content |
Dispersant content |
D50 (μm) |
Viscosity |
solvent |
TOB-KNG-CC503 |
15wt% |
0.25 wt% |
8.65 |
No Mobility |
Deionized water |
Micromorphology photo
SEM PHOTO
AFM PHOTO
Recommendation
- |
Applications |
||
Static conductive coating |
Conductive coating |
||
Dispersing time |
High speed shearing |
20-30 min |
20-30 min |
Emulsified |
20-30 min |
20-30 min |
|
Ball milling |
1-2 times |
1-2 times |
|
Added amount of graphene |
2-3wt% |
3-5wt% |